anode issmallerthan thecathodepittingelectron4used toremovecorrosion frommagnesiumpartsuniformsurfacetype ofcorrosionassociatedwith improperlycured primeranodedelaminationof the grainboundaries(looks likeflaking)neutrondue toimproperheattreatmentprotonmetal to jointcorrosion(also calledcrevicecorrosion)electropotentialdifferenceslowcorrosiontimecathodecorrosionaluminumoxide andiron oxidehydrogenembrittlementmethod ofpreventingstresscrackalodizedirect chemicalandelectrochemicalappears as awhite or graypowderydepositdrycorrosionionactive-passiveoxygen, andmetal ionrinsewithwateraromaticnaphtha2dissimilarmetalsappearsas areddishbyproductamalgamationcontact(conductivepath)goldwash with acommercialsolvent,decarbonize,and scrape witha grit blasterparalketoneboricacidAC43-4Aoxidationanodizemagnesiumbilgeanode issmallerthan thecathodepittingelectron4used toremovecorrosion frommagnesiumpartsuniformsurfacetype ofcorrosionassociatedwith improperlycured primeranodedelaminationof the grainboundaries(looks likeflaking)neutrondue toimproperheattreatmentprotonmetal to jointcorrosion(also calledcrevicecorrosion)electropotentialdifferenceslowcorrosiontimecathodecorrosionaluminumoxide andiron oxidehydrogenembrittlementmethod ofpreventingstresscrackalodizedirect chemicalandelectrochemicalappears as awhite or graypowderydepositdrycorrosionionactive-passiveoxygen, andmetal ionrinsewithwateraromaticnaphtha2dissimilarmetalsappearsas areddishbyproductamalgamationcontact(conductivepath)goldwash with acommercialsolvent,decarbonize,and scrape witha grit blasterparalketoneboricacidAC43-4Aoxidationanodizemagnesiumbilge

Corrosion & Cleaning - Call List

(Print) Use this randomly generated list as your call list when playing the game. There is no need to say the BINGO column name. Place some kind of mark (like an X, a checkmark, a dot, tally mark, etc) on each cell as you announce it, to keep track. You can also cut out each item, place them in a bag and pull words from the bag.


1
2
3
4
5
6
7
8
9
10
11
12
13
14
15
16
17
18
19
20
21
22
23
24
25
26
27
28
29
30
31
32
33
34
35
36
37
38
39
40
41
  1. anode is smaller than the cathode
  2. pitting
  3. electron
  4. 4
  5. used to remove corrosion from magnesium parts
  6. uniform surface
  7. type of corrosion associated with improperly cured primer
  8. anode
  9. delamination of the grain boundaries (looks like flaking)
  10. neutron
  11. due to improper heat treatment
  12. proton
  13. metal to joint corrosion (also called crevice corrosion)
  14. electro potential difference
  15. slow corrosion time
  16. cathode
  17. corrosion
  18. aluminum oxide and iron oxide
  19. hydrogen embrittlement
  20. method of preventing stress crack
  21. alodize
  22. direct chemical and electrochemical
  23. appears as a white or gray powdery deposit
  24. dry corrosion
  25. ion
  26. active-passive oxygen, and metal ion
  27. rinse with water
  28. aromatic naphtha
  29. 2 dissimilar metals
  30. appears as a reddish byproduct
  31. amalgamation
  32. contact (conductive path)
  33. gold
  34. wash with a commercial solvent, decarbonize, and scrape with a grit blaster
  35. paralketone
  36. boric acid
  37. AC 43-4A
  38. oxidation
  39. anodize
  40. magnesium
  41. bilge